clay insulating brick light weight (86) Online Manufacturer
Cold Crushing Strength: ≥3 MPa
Linear Change On Reheating,(5h,≤0.5 %): ≥1450 ℃
SiO2: 48%
Al2O3: 45%
Raw Material: Mullite
Al2O3: ≥42%
Bulk Density: ≤1.15 G/cm3
Cold Crushing Strength: ≥5 MPa
Bulk Density: ≤0.7 G/cm3
Cold Crushing Strength: ≥2.0 MPa
Cold Crushing Strength: ≥4.5 MPa
Linear Change On Reheating,(5h,≤2%): ≥1400 ℃
Product Description: Fireclay Refractory Brick Based On Chamotte, Fireclay, Ceramic Bond
Molding Method: Machine Pressed Brick
Al2O3: ≤1.0%
Fe2O3: ≤1.3%
Product Description: Fireclay Refractory Brick Based On Chamotte, Fireclay, Ceramic Bond
Al2O3: ≥42
Bulk Density: ≤1.3 G/cm3
Cold Crushing Strength: ≥5.0 MPa
Bulk Density: ≤1.2 G/cm3
Cold Crushing Strength: ≥4.5 MPa
Bulk Density: ≤1.2 G/cm3
Cold Crushing Strength: ≥4.5 MPa
Bulk Density: ≤1.3 G/cm3
Cold Crushing Strength: ≥5.0 MPa
Bulk Density: ≤0.8 G/cm3
Cold Crushing Strength: ≥3 MPa
Cold Crushing Strength: ≥3 MPa
Linear Change On Reheating,(5h,≤2%): ≥1250 ℃
Bulk Density: ≤1.2 G/cm3
Linear Change On Reheating,(5h,≤2%): ≥1350 ℃