90 high alumina bricks (62) Online Manufacturer
Thermal Shock Resistance: ≥15 Times
Application: High Temperature Furnaces And Kilns
Packaging Details: Pallet with seaworthy package
Delivery Time: 30
Apparent Porosity: ≤22%
Refractoriess: 1790℃
Packaging Details: Pallet with seaworthy package
Delivery Time: 15
Raw Material: Andalusite
Al2O3: ≥65%
Color: Ivery White
Al2O3: ≥40%
Refractoriness: SK36
Fe2O3: ≤2%
Refractoriness: SK38
Al2O3: ≥70%
Al2O3: ≥68%
Bulk Density: ≥2.4g/cm3
Raw Material: Flint Clay
Al2O3: ≥55%
Colar: Red
Shape: Standard Or Special Shape
Raw Material: Bauxite
Refractoriness: ≥1790
Raw Material: Bauxite
Al2O3: ≥55%
Apparent Porosity: ≤23%
CCS: ≥40Mpa